Quote:
Originally Posted by DaveWM View Post
Pretty sure how rebuilder did it has come up before. that have industrial size ovens that can heat up the entire tube very evenly, to the point where the glass just lifts off.
Sony even patented the process. Rauland had been using it for years, but never sought a patent. I don't know if there was ever a patent fight, but both of them used the same process - heat it up.

PVB used in the first rectangular tubes is impervious to water. I'm sure that if someone knew the exact brand of PVB, a solvent is readily available - whether it be ammonia, acetic acid, some alcohol based solvent, or some hydrocarbon solvent.

The same PVB is used with early automobile windshields where they bonded the safety glass to the oven glass and needed an optically clear adhesive.

https://en.wikipedia.org/wiki/Polyvinyl_butyral
__________________
Brian
USN RET 22YRS (Avionics/Cal)
CET-Consumer Repair and Avionics ('88)
"Capacitor Cosmetologist since '79"

When fuses go to work, they quit!