Clinton Electronics used to rebuild CRTs, but the cost was $350. That included new phosphor, aluminizing, the works. I was discussing the possibility of rebuilding & aluminizing a metal 16GP4 with one of their "seasoned" guys, and he said he would give it his best shot. He said it would have been a very difficult process, because the phosphor gets coated with laquer before it gets aluminized, to protect it. The laquer is normally removed during final evacuation, but is more difficult on metal tubes, due to the sharper corners. Also, metal tubes have a higher risk of imploding during final evacuation. The cost would have been the same, and if the rebuild wasn't successful, there would be no charge. How about that?? I was ready to do it, because aluminized 16GP4s don't exist, and this was when NOS 16GP4s were still bringing north of $300 on f-bay. This was right when they got bought out, and the new owners said "hell no" to metal CRTs.
They also bumped the price to $750++ for glass CRTs. Oh, well...
http://www.clinton-vdc.com/history.shtml
.