Quote:
Originally Posted by VintagePC
I wonder if it would be as effective to carefully go in with a thin needle and force a bit of water water into the cataract? It would probably be quicker than waiting for it to soak in by itself.
|
yes indeed. the problem seems to be the bonding agent often gets very hard when it turns milky white (RCA CRT's) On these it may take a hard pic like tool to work your way in. I was planning on doing just that to create cavities for chop stick insertion (slow pressure approach).
so now lets have some fun under the main heading of DE-CATing
1) COTL for chip off the glass, get medieval on its glass... lens that is
2) HOTL for heat off use the heat gun, have your insurance up to date
3) PLHMT for pressure, low heat, med time use wedges and unconcentrated solar heat
4) FOWWLT for float of with water long time, let the water slowly break down the bond
Recommneded are FOWWLT if you have time, and PLHMT if you are somewhat in a hurry, COTL and HOTL are only mentioned so they may be known of and avoided.
perhaps some better acronymn's can be developed that will sound snappier.
pretty sure the PLHMT would be best with zenith (gooey) CRT's
I have left of the use of a cutting wire (heated or not) as not sure its needed but maybe should be included as a zenith option
5)COWZO for cut off wiire zenith only... I like the sound of that one