Findm's story about the etched tv screen reminded me of a lab I worked at. Back in the storage room, we had a couple of specialty cabinets, including the blast proof metal cabinet, and a wooden one with metal hinges where we stored corrosives (18M HCl and HF acid, for instance). Well, the crap in that cabinet was impossible to keep, it would dissolve the caps to the bottles they were kept in, badly etch nearby glass containers, and most dramatically, dissolve the hinges on the storage cabinet itself!