I think they started using a different bonding material around the CTC-40 era. I have a CTC-40 with the original HiLite CRT and the bonding agent is perfect! Then I have a CTC-17 with a replacement colorama CRT from 1980 and it's perfect too, but then I have a Maggie from 68, and the CRT was replaced in 69, and, green halo. It's almost like somewhere between 1969 and 70 they used a different bonding agent. Correct me if im wrong of course.